版权说明 操作指南
首页 > 成果 > 详情

Effects of silane additives on corrosion resistance and durability of mortar

认领
导出
反馈
分享
QQ微信 微博
成果类型:
期刊论文
作者:
Liu Jiesheng*;Gong Xiaoqiang;Li Faping;He Xiang;Zhang Rongtang
通讯作者:
Liu Jiesheng
作者机构:
[Li Faping; Liu Jiesheng; He Xiang; Zhang Rongtang; Gong Xiaoqiang] Wuhan Polytech Univ, Sch Civil Engn & Architecture, Wuhan, Hubei, Peoples R China.
通讯机构:
[Liu Jiesheng] W
Wuhan Polytech Univ, Sch Civil Engn & Architecture, Wuhan, Hubei, Peoples R China.
语种:
英文
关键词:
Additives;Corrosion resistance;Corrosive effects;Coupling agents;Corrosion behavior;Distilled water;Fine aggregates;Fineness modulus;Mortar properties;Reference samples;Silane coupling agent;Water/cement ratio;Mortar
期刊:
MATERIALS PERFORMANCE
ISSN:
0094-1492
年:
2018
卷:
57
期:
3
页码:
42-45
基金类别:
This work was supported by the Na tional Natural Science Foundation of China (51409203). The authors express their great appreciation of the funding supported by Research and Innovation Initiatives of WHPU (2015d3) and State Key Laboratory of Silicate Materials for Architectures (Wuhan University of Technology SYSJJ201613).
机构署名:
本校为第一且通讯机构
院系归属:
土木工程与建筑学院
摘要:
A study was conducted to verify the validity of silane as an additive by monitoring the corrosion behavior of silane-enhanced mortar. Silane coupling agents were used in varying proportions, and the effect of the coupling agent content on mortar properties was studied. The integral silane mortar additive was (γ-glycidoxypropyl) methyldimethoxysilane (KH560). River sand with a fineness modulus of 2.43 was used as the fine aggregate. A water/cement ratio of 0.4 was used for preparing mortar mixtures incorporating no silane (the reference sample), and...